数字: 1.4005,电磁不锈钢易削性能
|
|
|
|
|
|
|
|
|
|
分类: 马氏体电磁不锈钢
|
|
|
|
|
|
|
|
|
|
密度: 7.7 克/厘米3
|
|
|
|
|
|
|
|
|
|
标准:
|
|
|
|
|
|
|
|
|
|
EN 10088-3:2005 不锈钢。一般用途耐蚀钢半成品、棒材、线材、型材和光亮产品交货技术条件
|
|
|
|
|
|
|
|
|
|
EN 10088-1:2005 不锈钢。不锈钢一览
|
|
|
|
|
1.4005对应牌号:
|
|
|
|
|
|
|
|
|
|
国标GB-T标准:数字牌号:S41617、新牌号:Y12Cr13、旧牌号:Y1Cr13,
|
|
|
|
|
|
|
|
|
|
美标:ASTMA标准:S41600 ,SAE标准:51416,UNS标准:416,
|
|
|
|
|
|
|
|
|
|
日标JIS标准:sus416,
|
|
|
|
|
|
|
|
|
|
德标DIN标准:1.4005,
|
|
|
|
|
|
|
|
|
|
欧标EN标准:X12CrS13。
|
|
|
|
|
|
|
|
|
|
化学成分:
|
|
|
|
|
|
|
|
|
|
碳 C:≤0.15
|
|
|
|
|
|
|
|
|
|
硅 Si:≤1.00
|
|
|
|
|
|
|
|
|
|
锰 Mn:≤1.00
|
|
|
|
|
|
|
|
|
|
磷 P:≤0.045
|
|
|
|
|
|
|
|
|
|
硫 S:0.15~0.25
|
|
|
|
|
(1.4005)的力学性能
|
|
|
|
|
|
|
|
|
|
Rm - 抗拉强度 (MPa) (+QT650) 650-850
|
|
|
|
|
|
|
|
|
|
[R P0.2 0.2% 屈服强度 (MPa) +QT650 450
|
|
|
|
|
|
|
|
|
|
A - 好小。断裂伸长率 (%) (+QT650) 12
|
|
|
|
|
|
|
|
|
|
布氏硬度(HB):(+A) 220
|
|
|
|
|
|
|
|
|
|
1.4005热处理:
|
|
|
|
|
|
|
|
|
|
硬度HBW≤:退火200,淬火回火159,硬度HRB≤:93,
|
|
|
|
|
|
|
|
|
|
加热温度:800~900,
|
|
|
|
|
|
|
|
|
|
加热方式:空冷或缓冷。
|
|
|
|
|
|
|
|
|
|
1.4005应用领域:用于自动车床加工的零件和标准件,如螺栓,螺帽等。
|
|
|
|
|
|
|
|
|
|
铬 Cr:12.00~13.00
|
|
|
|
|